Metal roof restoration · Anti-rust

Rusty metal roof? Don't re-roof yet.Restoration typically costs 40–60% of re-roofing

Our patented rust converter primer turns tightly adhered rust into a stable protective layer — no sandblasting, no stripping the roof. Only sheets that have rusted through are replaced. We work from the outside of the roof, area by area, while production continues.

  • Patented rust converter — no sandblasting
  • Number of coats set by rust level
  • Full system tested: 300 h salt spray, 7 MPa adhesion
  • If it's time to re-roof, we say so
40–60%
of the cost of re-roofing
7 MPa
adhesion, full system (third-party tested)
300 h
neutral salt spray, no defects
Patent
ZL201910886793.4 rust converter

Whole factory roofs restored — not one sheet replaced

Same roof before and after, photographed by our own crews. Work done from the outside of the roof while the factories kept running.

  • Manufacturing plant · Huangshi, Hubei – BeforeBefore Manufacturing plant · Huangshi, Hubei – AfterAfter

    34,800 m²

    Manufacturing plant · Huangshi, Hubei

    Several large-span buildings · 2024

    Old roofs faded with patches of rust. Fully recoated in bright blue — no sheets replaced.

  • Shiji Xingui Ceramics · Yichun, Jiangxi – BeforeBefore Shiji Xingui Ceramics · Yichun, Jiangxi – AfterAfter

    52,000 m²

    Shiji Xingui Ceramics · Yichun, Jiangxi

    Ceramics factory · 2022

    Red-brown roof sheets rusted and faded. Rust converter primer, then a dark blue-grey topcoat over the whole roof.

  • Xiduan Machine Tools · Wuxi – BeforeBefore Xiduan Machine Tools · Wuxi – AfterAfter

    12,000 m²

    Xiduan Machine Tools · Wuxi

    Machine tool plant · 2020

    Rust spots everywhere and some perforations. Perforations patched, rust converted, then primer and a white topcoat — rust protection and cooling in one job.

Which rust level is your roof?

One roof often has all three. We grade it area by area on site and specify each area separately.

  1. Light rust

    Light rustRestore directly

    Scattered rust spots at fasteners, folds and sheet backs; the surface is still fairly smooth.

    Pressure-wash off loose rust and flaking paint, then 1–2 coats of CST880-701 2-in-1 rust primer & topcoat.

    CST880-701 ×1–2

  2. Medium rust

    Medium rustSeal, then topcoat

    Original paint chalked and discoloured over large areas, with joined-up rust patches; surface still basically flat.

    After removing loose rust: 2 coats of RPP210 rust-tolerant primer to seal the rust, then 1–2 coats of CST880 topcoat.

    RPP210 ×2 → CST880 ×1–2

  3. Heavy rust

    Heavy rustConvert + protect + topcoat

    Whole surface rusted; laps and sheet edges often rusted through; rough, gritty rust.

    Remove loose rust, 1 coat of MAP120 rust converter, 2 coats of RPP210, then 1–2 coats of CST880. Perforated sheets are patched or replaced first.

    MAP120 ×1 → RPP210 ×2 → CST880 ×1–2

If sheets are rusted through over large areas or purlins are corroded, re-roofing is better value, and we'll tell you.

Why the rust doesn't need grinding off

  1. 1

    Tight rust is converted where it is (patented)

    MAP120 reacts with the rust to form a dense, stable black protective layer. No sandblasting, no grinding to bare metal — old sheets don't get thinner (patent ZL201910886793.4).

  2. 2

    Fasteners and laps: fabric-reinforced, three coats

    Rust starts at screws, laps and gutters — the same places that leak. Each one gets a coat, a polyester fabric, then two more coats. A bead of sealant alone cracks within a year or two.

  3. 3

    Primer to topcoat from one factory

    Rust converter, rust primer and topcoat are all made in our factory and tested together: the CST880 system has 7 MPa adhesion (CTC report WT2020B01C04598).

Rusty factory roof before restoration
Rusty factory roof before restoration

Restoration vs re-roofing

TEYISHU restorationNew roof sheets
CostTypically 40–60% of re-roofing, depending on rust level and sheets replacedStrip-out, disposal, new sheets and installation
ProductionWork from the outside of the roof; production continuesRoof opened up; goods often moved, production stopped
ScheduleArea by area; just avoid rainy daysLong strip-and-fit programme; risky in the rainy season
LeaksRust, leaks and topcoat in one jobNew sheets still need screws and laps sealed

The price depends on rust level, the number of leak points (screws, laps, gutters, skylights), where the work is (roof, walls or steelwork) and the area and height.

Third-party test data: full anti-rust system (primer + topcoat)

Anyone can write "acid and salt-spray resistant". Ask for the report number, check that the whole system was tested, and look for hours and results.

TestStandard requirementTEYISHU result
Neutral salt spray300 h: no rust, blistering, cracking or peeling300 h, no defects
Acid resistance (sulphuric acid)48 h, no defects48 h, no defects
Alkali resistance (sodium hydroxide)48 h, no defects48 h, no defects
Water resistance96 h, no defects96 h, no defects
Continuous condensation120 h, no defects120 h, no defects
Pull-off adhesion≥ 3 MPa7 MPa
Adhesion after 300 h salt spray≥ 3.5 MPa6 MPa
Artificial weathering, 300 h≤ grade 1Grade 0

National Building Materials Testing Center (CTC Group), report WT2020B01C04598 — system tested to HG/T 5176-2017 (alkali resistance assessed at corrosivity category C4). All assessed items passed.

Buying the coatings for your own crew or your customers?

No MOQ on standard products, 20 kg pails, ships 3–5 days after payment. We specify the system, calculate quantities and train your applicators by video.

On projects we install

For projects in China, and for projects abroad installed by our own crew (where project size justifies it and local rules allow).

  • If it's time to re-roof, we say so We grade the rust and count rusted-through sheets, then price the restoration item by item. If the sheets are rusted through over large areas or the purlins are corroded, re-roofing is better value and we tell you.
  • Rust removal, coats and film thickness in the contract Each layer — which product, how many coats, what thickness — is written into the quote and the contract.
  • Final payment after acceptance Checked against the agreed steps and film thickness before the final payment.
  • No shutdown Work from the outside of the roof, area by area. Production carries on.
  • 5-year warranty covers re-rusting Re-rusting, peeling and flaking are all covered — materials and labour. Before/after photos and film-thickness records come with the handover documents.
  • Buying coatings only? 5-year limited material warranty on complete TEYISHU systems, applied according to our instructions.

Questions buyers ask

How much does metal roof restoration cost per m²?
It depends on rust level, the roof area to be treated, the number of leak points and the area and height. That's why we look at the roof first. Where the sheets have not rusted through over large areas, restoration typically costs 40–60% of re-roofing. Coatings for your own crew are quoted per order.
The rust is really bad. Can it still be restored?
Yes, as long as the sheets have not rusted through over large areas. Perforated sheets are patched or replaced first, then MAP120 + RPP210 + CST880. If the sheets are widely perforated or the purlins are corroded, re-roofing is better value and we'll tell you.
Do we have to sandblast or grind to bare metal?
No. Remove loose rust and flaking paint by pressure-washing and scraping; the converter primer goes straight onto the remaining tight rust. Sheets don't get thinner and there is no grinding dust on the roof.
What colours are available?
CST880 and CST880-701 come in sea blue, mid grey and white-grey as standard; other colours to a colour card on request.
Can we combine rust restoration with a cool roof?
Yes. The rust system goes underneath and the 901/902 cool roof coats go on top. See Complete Roof Restoration.
What are the application conditions?
Apply at 5–35 °C and relative humidity up to 85%, with the surface at least 3 °C above the dew point and no hotter than 50 °C (avoid midday heat in summer). Do not apply in rain, fog or wind of force 5 or more, or on a wet surface; keep rain off for 4 hours after application (at 25 °C).

Send roof photos — we'll tell you if it can be restored

Tell us what you need. Photos of the roof help us answer faster.

  • Project enquirySend a few roof photos and the area. We'll tell you whether it can be restored, roughly what rust level it is, and whether any sheets need replacing.
  • Product enquiryKnow the product? Ask for a price. Not sure? Tell us the use and the area and our engineers will specify it.

We reply by email within one working day.

I need
Problem (tick all that apply)
Tap to choose photos, or drag them here

We use your details only to answer this enquiry.