Heat, rust and leaks in one job
Hot, rusty and leaking?Fixed in one mobilisation, by one team
One survey, one quote and one crew for rust treatment, leak sealing and a cool roof topcoat — all coatings from the same factory. Only perforated sheets are replaced. At Shaanxi Baoguang, workshop air dropped 12.4 °C after the partly rusted roof was restored.
- Rust, leaks and heat in the right order
- Perforated sheets replaced locally, not the whole roof
- All layers from one factory — compatible
- No shutdown
- ↓12.4 °C
- workshop air, Shaanxi Baoguang (45.9 → 33.5 °C)
- ↓41.5 °C
- roof surface, Shaanxi Baoguang (77.5 → 36.0 °C)
- 1 team
- from survey to handover
- Outside
- roof work, area by area
The order of work: rust → leaks → cool roof
The cool roof topcoat works by reflecting sunlight, so it must be the outermost layer. Rust and waterproofing go underneath, and the topcoat protects them.
- 01
One survey
Rust levels, leak points and sheets to replace marked area by area; temperatures recorded before work.
- 02
Wash and replace sheets
Pressure-wash off loose rust, chalking and oil; rusted-through or deformed sheets replaced or patched.
- 03
Rust layer
By rust level — light: CST880-701 ×1–2; medium: RPP210 ×2; heavy: MAP120 ×1 + RPP210 ×2.
- 04
Seal the joints
Every screw sealed; laps, gutters, skylights and fan bases with AEW320 fabric-reinforced 3-coat seal.
- 05
Cool roof layer
901 primer and 902 topcoat, 1–2 coats each; TIC610 mid-coat added where more insulation is needed.
- 06
Handover
Coating and joints inspected, temperatures re-measured at the agreed points, water test or rain check, then the final payment.
Before and after: rust, leaks and heat in one job
-
Before
After
43.7 → 36.5 °C
Yuanda Metal (Shenzhen)
Rusted arched metal roof · 4,800 m² · 5 days
Rust treatment, joint sealing and cool roof coats. Workshop air 43.7 °C → 36.5 °C; roof surface 72.6 °C → 46.1 °C.
-
Before
After
42.8 → 34.8 °C
Foshan Huahe Stainless Steel Pipe
Heavily rusted curved roof · 9,680 m² · 12 days
RPP210 rust primer and 902 cool roof topcoat over the whole roof. Workshop air 42.8 °C → 34.8 °C; roof surface 74.3 °C → 38.3 °C.
Measured results on restored roofs
-
↓12.4 °C workshop air
45.9 °C 33.5 °C
Shaanxi Baoguang Auto Parts · Baoji
9,000 m² · 7 days · 2026
Roof surface 77.5 °C → 36.0 °C
-
↓7.2 °C workshop air
43.9 °C 36.7 °C
Baoguang (Tianjin) Auto Parts
24,000 m² · 14 days · 2026
Roof surface 73.9 °C → 36.8 °C
-
↓8.0 °C workshop air
42.8 °C 34.8 °C
Foshan Huahe Stainless Steel Pipe
9,680 m² · 12 days · 2017
Roof surface 74.3 °C → 38.3 °C
How we measure: indoor air at about 1.5 m above the floor, before work and after completion on a day with similar weather; roof surface with an infrared thermometer. Results differ from building to building — heat sources, ventilation and roof type all matter.
Priced item by item — on one quote
| Item | What decides the cost |
|---|---|
| Washing and preparation | Roof area, rust and dirt; one mobilisation means one wash |
| Sheet replacement and rust layer | Number of rusted-through or deformed sheets; rust level decides CST880-701, RPP210 or MAP120 + RPP210 |
| Joint sealing | Number and length of screws, laps, gutters and skylights, listed separately |
| Cool roof layer | Roof area and cooling target; standard system or with TIC610 mid-coat |
Do you have to do all three? No. Areas that are rusty but not leaking skip the waterproofing; areas that only need rust protection skip the cool roof. The quote lists each area and step, so you can choose item by item.
Questions buyers ask
How much cooler will the workshop be after restoration?
Is doing it all at once cheaper than separately?
Can production carry on?
The rust is very bad. Can it still be done?
Can we buy the full set of coatings for our own contractor?
Send roof photos — heat, rust and leaks assessed together
Tell us what you need. Photos of the roof help us answer faster.
- Project enquirySend a few roof photos and the area. We'll tell you which of the three the roof needs, which it doesn't, and how we'd do it.
- Product enquiryKnow the product? Ask for a price. Not sure? Tell us the use and the area and our engineers will specify it.
We reply by email within one working day.